Dobra Warstwa

Defect or normal 3D printing?

We make every print from your file and the settings you choose in the quote. Here you'll see what a correct print looks like, what we're responsible for and what comes from the design, the settings or how the print is used.

Three possible answers

If something about your print worries you, it almost always fits one of these groups. You'll see the same icons throughout this page.

Normal for 3D printing

This is what a correct 3D print looks like. It comes from the technique itself: the plastic is laid down layer by layer.

  • visible layer lines
  • a seam where each layer starts
  • small marks left by supports
  • dimensions usually within ±0.2 mm

Not a defect and not covered by a complaint.

Production fault

Something went wrong on our side: during printing, finishing, packing or shipping.

  • a different material, colour, scale or quantity
  • layers splitting, cracks or warping from day one
  • holes, shifted layers, a missing part of the model
  • a print damaged in transit

We reprint or repair it. We cover the costs and the shipping.

Your choice

A result of the file's design, the settings chosen in the quote or how the print is used.

  • walls too thin or no clearance in the design
  • a crack with low infill or the wrong orientation
  • sagging overhangs with supports turned off
  • PLA that softened in a hot car

Not a print defect. We're happy to help you choose better settings next time.

How we assess a complaint

We look at every report individually – photos are usually enough. We check four things in order.

  1. 1

    Is the print different from the order?

    Material, colour, quantity, scale, a missing part of the model.

    YesProduction fault

  2. No

    2

    Did it arrive damaged or badly made?

    Layers splitting, cracks, warping, holes, shifted layers, a crushed parcel.

    YesProduction fault

  3. No

    3

    Does the problem come from the file, the settings or the way it's used?

    A wall too thin in the design, too little infill for the load, supports turned off, PLA in a hot car.

    YesYour choice

  4. No

    4

    None of the above?

    Layer lines, a seam, small support marks and deviations up to ±0.2 mm are how a print normally looks.

    Normal for 3D printing

If a defect shows up within 2 years of delivery, we assume it was there from the start – unless it clearly comes from something else: the design, the settings or the way the print was used. Not sure which group your case fits? Write to us.

Normal for 3D printing

This is what a correct print looks like

We print using FDM: a nozzle lays down melted plastic in thin lines, layer by layer. You'll see these traces of the technique on every print, from any print shop.

Layer lines

Fine horizontal lines show on the sides. The thicker the layer you choose in the quote, the more visible they are.

0.08 mm – barely visible · 0.28 mm – clearly visible

Steps on curves

Rounded and gently sloping surfaces, such as the top of a dome, are made of small steps. They're most visible at the top.

Seam

Every layer starts and ends somewhere. That leaves a vertical line of small bumps, usually hidden on an edge of the model.

Support marks

We remove supports before shipping. Where they touched, the surface stays rougher. Easy-release supports leave fewer marks.

Dimensional deviations

Dimensions can differ from the file, usually by up to ±0.2 mm. Large flat parts can differ a little more, because plastic shrinks as it cools.

Shade and gloss

Colours look different on screen than in real life, and material batches can differ slightly in shade. The sides and the top can have a different gloss.

The bottom takes on the texture of the print bed and looks different from the sides.

The inside isn't solid. It has infill, e.g. 20%, so the part is lighter than a casting.

Bridges, meaning horizontal spans over empty space, can sag slightly underneath.

TPU is flexible and has less precise bridges and overhangs than rigid materials.

Production fault

What we're responsible for

A print must match your file and the settings in your order, and be fit for the usual uses of its material. If it isn't, that's our fault and we fix it at our cost.

Doesn't match the order

A different material, colour, scale or quantity than you ordered.

Part of the model missing

A section that is in the file and is at least about 0.8 mm thick is missing.

Splitting or cracking

Layers come apart on their own or with light finger pressure, or the crack was there from day one.

Warping

The print arrived bent or with its corners lifted so that it doesn't lie flat.

Shifted layers

Part of the model is offset from the rest. There's a clear step across the whole print.

Holes and under-extrusion

Gaps in the walls, missing lines, see-through spots where the file has a solid wall.

Supports left on

Supports were left in places they could have been removed from.

Damaged in transit

The print arrived broken or crushed. Take photos of the parcel as soon as you receive it.

2 years
we're responsible for defects that show up within this time from delivery
14 days
to answer your complaint – if we don't, it's accepted
PLN 0
is what a reprint or repair costs you, shipping included
Photos
are usually enough – you only send the print back if we ask
Your choice

Quote settings and what they change

You choose the print settings in the quote, and we print with exactly those settings. Whatever results from them isn't a print defect. It's usually about strength and appearance.

Orientation decides where a part breaks

Layers bond to each other less strongly than the material itself. The same part, printed in a different orientation, can be several times weaker.

Lying flatlayers run along the beam – it holds
Standing uplayers run across – it breaks between them

Same shape, same material. You choose the orientation in the quote preview – rotate the model so the load doesn't pull the layers apart.

Walls add more strength than infill

When a part bends, the outer walls do most of the work. The inside carries much less, so adding infill alone soon stops helping.

2 walls · 10%Light and cheap. For decorations and figurines.
4 walls · 40%For holders, hooks and parts that carry a load.

Material

PLA · PETG

What it changes

Resistance to heat, impact and sunlight, and whether the part is stiff or flexes.

Not a defect when

a PLA holder softened in a hot car or broke after falling onto tiles.

Infill

from 10% (light) to 100% (solid)

What it changes

Weight, stiffness and how much the inside of the part can take.

Not a defect when

a bracket with 10% infill broke under a heavy load.

Walls

from 2 to 6, depending on the nozzle

What it changes

Above all, bending strength, plus water-tightness and room for sanding.

Not a defect when

the infill shows through after sanding, or a part with 2 walls cracked when bent.

Layer height

from 0.06 to 0.36 mm

What it changes

How smooth the sides and curves are, the print time and the price.

Not a defect when

at 0.28 mm the layers are clearly visible and a dome has visible steps.

Nozzle

0.2 · 0.4 · 0.6 mm

What it changes

The smallest detail that will come out, as well as strength and print time.

Not a defect when

1 mm high lettering printed with a large nozzle is unreadable.

Orientation

from the file · rotated · laid flat

What it changes

The direction of the layers, meaning where the part is weaker, and which surfaces get supports.

Not a defect when

a hook printed standing up broke along a layer.

Supports

automatic · off · standard · easy-release

What it changes

How the underside of overhangs and areas over empty space look.

Not a defect when

without supports an overhang sagged and has a ragged underside, or standard supports left small marks.

Scale

in percent

What it changes

The thickness of walls and details, hole diameters and the fit with other parts.

Not a defect when

after scaling down to 50% a 1.2 mm wall became 0.6 mm and came out brittle or full of holes.

The quote warns you when a model has overhangs and supports are off, or when a model doesn't fit in the printer. If we see while checking the file that the model won't print with your settings, we'll write to you before printing.

Your choice

Heat: the most common cause of warping

Every plastic softens above a certain temperature. A print that deformed in the heat isn't defective – it went past the limit of its material. The values are approximate.

60 °C100 °C
PLA55 °C
PETG70 °C

The temperature at which a print starts to soften under load. The line at 60 °C is a car heated by the sun (it can get hotter), at 100 °C boiling water.

A car dashboard in the sun gets hotter than the inside of the car, and a dishwasher washes at up to about 70 °C.

Your choice

The file's design

We print the model exactly as it is in the file. We don't fix the design or change its dimensions unless we agree on it with you. You're responsible for the design: dimensions, tolerances, strength and fit with other parts.

≥ 0.8 mm

Walls and details

Thinner features may not print or may come out brittle. Make them thicker in parts that carry a load.

0.2–0.4 mm

Clearance in fits

Design parts that need to fit together with some clearance. Without it, they may not go into each other.

Ø

Holes

Small holes usually come out slightly tighter. Leave some extra room for screws and pins, or drill them out after printing.

mm

Units and dimensions

The file must be in millimetres. You can see the dimensions after scaling in the quote – check them before ordering.

R

Corners and narrow sections

Sharp inside corners and thin joints are the first to crack. Round them off in the design.

STL · 3MF

Watertight mesh

The model can't have holes in its mesh. We check the file before printing and write to you if something's wrong.

Your choice

Use

We're not responsible for damage caused by using a print beyond what its material can handle.

°C

Heat

A hot car, a windowsill in full sun, a radiator, boiling water, a dishwasher. Above the material's limit, the print softens and changes shape.

kg

Load and impact

More load than the part can take, a fall, a knock. PLA is stiff but brittle.

days

Constant pressure

Under a long-term load plastic slowly bends, and faster when it's warm.

UV

Sun and weather

Outdoors, PLA and ABS fade and become brittle over time. ASA works better in the garden.

chem

Solvents

Acetone dissolves ABS and ASA. Wash prints by hand in lukewarm water with a mild detergent.

tools

Sanding, drilling, gluing

Finishing, painting and driving screws in without a prepared hole are at your own risk.

no

Excluded uses

Prints aren't meant for contact with food, for medical use or for parts that someone's safety depends on.

< 3 yrs

Small parts

Prints aren't toys. Keep small parts away from children under 3.

How to tell similar cases apart

The same symptom can have different causes. What matters is when and in what conditions the problem appeared.

A crack along the layers

Production fault

The layers come apart with light finger pressure, or the crack was visible as soon as you unpacked it.

Your choice

It broke under a load or after a knock, and the part was oriented so that the load pulled the layers apart.

Warping

Production fault

The print arrived bent or with corners lifted off the surface.

Your choice

It bent later in a hot car, near a radiator or in a dishwasher.

Underside of an overhang

Production fault

Supports were on, but the overhang has holes, broke off or still has supports attached.

Your choice

Supports were off and the underside sagged or is ragged.

Dimensions

Production fault

The scale is different from the order, or a dimension differs from the file by clearly more than ±0.2 mm (apart from large flat parts).

Your choice

The part doesn't fit another one because the design had no clearance, or the hole is exactly the diameter of the screw.

Surface

Production fault

A step across the model, holes in a wall, clear bands of missing material.

Normal for 3D printing

Even, regular layer lines, steps on curves, a seam, small support marks.

Colour

Production fault

The print is a different colour from the one in your order.

Normal for 3D printing

The shade is slightly different from the screen or from a previous order.

Before you order

Most problems in the “Your choice” group can be avoided in the quote.

  • Match the material to where it'll be used. Don't choose PLA for a car, direct sun or outdoors. Choosing a material
  • Will the part carry a load? Add walls and orient it so the load runs along the layers instead of pulling them apart.
  • Check the dimensions and scale in the quote preview, especially after changing the scale.
  • Don't turn supports off if the quote shows that the model has overhangs.
  • Describe how it'll be used in the order notes, or write to us before ordering if the part has to carry a heavy load. We'll help you choose the material and settings.
Settings for typical parts
PartWallsInfillOrientation
Figurine, decoration210–15%any
Enclosure, organiser2–320%bottom down
Holder, hook420–40%on its side
Gear4–640%flat
TPU seal2100%flat
Production fault

How to make a complaint

Just send an email to kontakt@dobrawarstwa.pl.

  1. 1

    Write to us

    Give your full name, order number, a description of the problem, the date you noticed it and what you'd like: a reprint, a repair, a price reduction or a refund.

  2. 2

    Attach photos

    The whole print and a close-up of the defect. For transit damage, also the parcel and the label, and for dimensions – the print next to a ruler or calipers.

  3. 3

    Keep the print

    Don't send it back until we ask. If we need it, we'll tell you how to send it and pay for the shipping.

  4. 4

    Wait for our answer

    We'll reply within 14 days. Once a complaint is accepted, we reprint or repair the part, usually within our standard production time.

This page sums up sections 8, 9 and 12 of our Terms and conditions in plain language. The Terms are binding, and this page doesn't limit your rights as a consumer. The complaint form and deadlines are on the Complaints page (in Polish).